Surface Preparation: Concrete shall be in place for 7 days minimum. Substrate must be completely dry.
Surface shall have a smooth finish free of voids, sharp protrusions, laitance and form release agents.
Block or brick walls shall have mortar joints struck flush.
• Primer: Surfaces to receive Strip-N-Flash™ must be clean and dry. For best results, concrete, masonry
and some exterior gypsum substrates require coating with Primer. Apply Primer per manufacturer’s
recommendations.
• Application: Precut Strip-N-Flash™ to fit each location. Remove siliconized release liner and position
membrane carefully before pressing in place. Press firmly in place with a steel hand roller, taking care to
avoid air pockets and wrinkles. Overlap adjoining pieces 2 inches. Cut bottom edge back 1/2 inch from
exterior surface of building and place on drip edge. Be sure Strip-N-Flash™ is installed a minimum of
four-inches above the mortar deflection.
• Terminations: Press termination edges firmly in place with a hammer handle or similar tool. The use of
a surface mounted termination bar or placing the flashing membrane into a joint of the inner back up
wall is recommended for vertical terminations. ABP End Dams are recommended at horizontal
terminations.
Note: Failure to use adequate pressure at terminating edges will result in a poor seal and a potential
leak.
Cop-R-Shield PC
Cop-R-Shield™ PC is our non-asphaltic copper flashing, ideal for deck construction and termite shield
protection. The product should be installed with the copper side facing the plywood sheathing and the
poly facing out.