Granite
rough 21 LLW 0.879 8
Granite rough, 4 different
samples
70
SW
0.95–0.97 9
Granite rough, 4 different
samples
70 LW 0.77–0.87 9
Gypsum
20 T 0.8–0.9 1
Ice: See Water
Iron and steel cold rolled 70
SW
0.20 9
Iron and steel cold rolled 70 LW 0.09 9
Iron and steel covered with red
rust
20 T 0.61–0.85 1
Iron and steel electrolytic 100 T 0.05 4
Iron and steel electrolytic 22 T 0.05 4
Iron and steel electrolytic 260 T 0.07 4
Iron and steel electrolytic, care-
fully polished
175–225 T 0.05–0.06 1
Iron and steel freshly worked
with emery
20 T 0.24 1
Iron and steel ground sheet 950–1100 T 0.55–0.61 1
Iron and steel heavily rusted
sheet
20 T 0.69 2
Iron and steel hot rolled 130 T 0.60 1
Iron and steel hot rolled 20 T 0.77 1
Iron and steel oxidized 100 T 0.74 4
Iron and steel oxidized 100 T 0.74 1
Iron and steel oxidized 1227 T 0.89 4
Iron and steel oxidized 125–525 T 0.78–0.82 1
Iron and steel oxidized 200 T 0.79 2
Iron and steel oxidized 200–600 T 0.80 1
Iron and steel oxidized strongly 50 T 0.88 1
Iron and steel oxidized strongly 500 T 0.98 1
Iron and steel polished 100 T 0.07 2
Iron and steel polished 400–1000 T 0.14–0.38 1
Iron and steel polished sheet 750–1050 T 0.52–0.56 1
Iron and steel rolled sheet 50 T 0.56 1
Iron and steel rolled, freshly
20 T 0.24 1
Iron and steel rough, plane
surface
50 T 0.95–0.98 1
Iron and steel rusted red, sheet 22 T 0.69 4
Iron and steel rusted, heavily 17
SW
0.96 5
Iron and steel rusty, red 20 T 0.69 1
Iron and steel shiny oxide layer,
sheet,
20 T 0.82 1
Iron and steel shiny, etched 150 T 0.16 1
Iron and steel wrought, carefully
polished
40–250 T 0.28 1