instructions on the back of the Restore Deck Stripper label before proceeding. Next sand the entire deck using 50
or 60 grit sand paper. This will open the pores of the wood and create a textured surface that is easier for the
coating to adhere to.
Step 2 Clean:
Clean the surface using a deck brush and the Restore Deck & Concrete Cleaner. The surface must be completely
clean and free of dirt, grease, mildew and organic growth to ensure product bonding and adhesion. For best
results use a pressure washer, in addition to the Restore Deck & Concrete Cleaner, to remove embedded dirt and
grime. (Use at a low setting 500-1200 PSI. Do not use high pressure as it may harm the wood.) For mildew and
other organic growth use a diluted solution of household bleach (3 parts water to 1 part bleach) applied to the
surface before cleaning. Loose paint needs to be scraped and removed from the surface.
Step 3 Test Surface for Application:
AFTER CLEANING THE SURFACE YOU MUST CONDUCT A SPLASH TEST TO ASSURE THE OLD COATING IS FULLY
REMOVED FOR PROPER ADHESION OF THE NEW TOPCOAT. PREVIOUSLY APPLIED SEALERS may be present on the
deck and are not always visible. Conduct a splash test by sprinkling water on multiple areas of the surface. Check
at least 4 areas, or more for larger decks. Be sure to check both high traffic areas such as walkways and non-traffic
areas. If the water absorbs rapidly into the surface, the surface is ready to be coated. If the water beads, puddles
or is not absorbed, the surface is sealed and not ready to coat. If any part of the surface is not absorbing the
water, use the Restore Deck Stripper and sand using 50 or 60 grit sand paper again in that section. Clean again
with a brush and Restore Deck & Concrete Cleaner and conduct the splash test again. Continue this process until
the water is absorbed by the wood in all test areas. Let the surface dry completely before application. Failure to
follow this process will result in poor adhesion and possible coating failure.
Step 4 Light Repairs:
Raised nail heads and/or screws should be secured using a hammer or screwdriver. Remove loose splinters and
replace severely damaged or rotting boards. Fill larger cracks using RESTORE CRACK FILLER or a similar acrylic,
non-silicone filler. Allow to dry.
6. WEATHER
Monitor the weather to see not only what the weather will be like for the day you plan on applying Restore
Metallic Semi-Transparent Stain, but also for at least 2 hours after application is complete. ONLY APPLY RESTORE
METALLIC SEMI-TRANSPARENT STAIN WHEN THE AMBIENT TEMPERATURE WILL BE BETWEEN 50-90 DEGREES
FAHRENHEIT DURING APPLICATION AND FOR AT LEAST 2 HOURS AFTER APPLICATION. DO NOT APPLY IF RAIN IS
EXPECTED THE DAY OF APPLICATION OR WITHIN 24 HOURS OF COMPLETING THE APPLICATION.
7. APPLICATION
ONE COAT OF RESTORE METALLIC SEMI-TRANSPARENT STAIN IS REQUIRED
TRIM AND VERTICAL SURFACES
Before applying Restore Metallic Semi-Transparent Stain to the horizontal portions of the Deck, first coat vertical
surfaces such as deck posts, railings, or balusters. Next cut in around edges with a brush and coat visible areas
between deck boards.
STEP BY STEP INSTRUCTIONS FOR APPLICATION
STEP 1:
Before using Restore Metallic Semi-Transparent Stain, mix material thoroughly and repeat mixing occasionally
during application. When using more than one container, combine all containers to ensure color consistency.