- Graphite : Rat LD
50
2 mg/L/4hr (male/female) (OECD Guideline 403)
- Fe : Rat LC
50
100 mg/m³/6hr
- Dimethyl carbonate : Rat LD
50
5.36 mg/L/4hr (male/female) (OECD Guideline 403)
- Aluminum : Rat LC
50
0.888 mg/L/4hr (analytical) (OECD TG 403)
- 1,3-Dioxolan-2-one : Rat LC
0
= 730 mg/ /8hr
- Ethyl acetate : Rat LCL
0
6000 ppm (male/female)
- Carbon black : Rat LC
50
0.005 mg/L/4hr
- Lithium carbonate;Lithane : Rat LC
50
2 mg/L/4hr (male/female) (OECD Guideline 403)
- 1-Methyl-2-pyrrolidinone : Rat LC
50
5.1 mg/L/4hr (male/female) (OECD Guideline 403)
Skin corrosion/ irritation :
- Graphite : In the skin irritation test using rabbits, the test material was not irritating. (OECD Guideline
404, GLP)
- Fe : In test on skin irritation with rabbits, skin irritations were not observed.(Read across;
Fe3O4)(OECD TG 404, GLP)
- Copper : In test on skin irritation with rabbits, skin irritations were not observed. (OECD TG 404, GLP)
- Dimethyl carbonate : In the skin irritation test using rabbits, the test material was not irritating. (OECD
Guideline 404)
- Aluminum : Aluminium oxide caused slight erythema in 2/12 rabbits. The observed effects do not
lead to a classification. Aluminium oxide is, therefore, not considered to be a primary skin
irritant.(OECD TG 404)(Read across; aluminium oxide)
- Polyethylene : No irritation was observed at the other two treated sites and no corrosive effects were
noted during the study using rabbits. The primary irritation index was calculated as 0.2 and
polyethylene was classified as a mild irritant.
- 1,3-Dioxolan-2-one : In the skin irritation test using rabbits, the test material was not classified.
(OECD Guideline 404, GLP)
- Lithium hexafluorophosphate(1-) : In the skin irritation test using human, the test material was
corrosive. (EU Method B.40, GLP)
- Ethyl acetate : In the skin irritation test using rabbits, the test material was slightly irritating. (OECD
Guideline 404)
- Carbon black : In test on skin irritation with rabbits, skin irritations were not observed. (OECD TG 404)
- Nickel; Raney nickel : Industrial nickel dust causes nickel dermatitis.
- Lithium carbonate;Lithane : In the skin irritation test using rabbits, the test material was not irritating.
(OECD Guideline 404, GLP)
- 1-Methyl-2-pyrrolidinone : In the skin irritation test using rabbits, the test material was slightly
irritating. (OECD Guideline 404, GLP)
Serious eye damage/ irritation :
- Graphite : In the eye irritation test using rabbit, the test material was not irritating. (OECD Guideline
405, GLP)
- Fe : In test on eyes irritation with rabbits, eyes irritations were not observed.(Read across;
Fe3O4)(OECD TG 405, GLP)
- Copper : In test on skin irritation with rabbits, skin irritations were not observed. (OECD TG 405, GLP)
- Dimethyl carbonate : In the eye irritation test using rabbit, the test material was not irritating. (GLP)
- Aluminum : An eye irritation study of the aluminium oxide was performed in rabbits. No eye irritation/
corrosion effects were observed. (Read across; aluminium oxide)
- Polyethylene : Mild irritants were observed in eye irritation test with rabbits. (Score 11.7/110)
- 1,3-Dioxolan-2-one : In the eye irritation test using rabbit, the test material was moderately irritating.
(OECD Guideline 405, GLP)
- Lithium hexafluorophosphate(1-) : In the eye irritation test using fertilised brown leghorn chicken
eggs, the test material was severely irritating. (GLP)
- Ethyl acetate : In the eyes irritation test using rabbits, the test material was not irritating. (OECD
Guideline 405)