Product Specifications
Doc. No.
Q/WAPL503562-1011
Edition No.
1.0
Polymer Lithium-ion battery
Product Specification
8/10
Battery pack should have sufficient strength and battery should be protected from
mechanical shock. No sharp edge components should be inside the pack contains the battery.
9.2 PCM design
The overcharge threshold voltage should not be exceeding 3.95V.
The over-discharge threshold voltage should not be lower than 2.3V.
The PCM should have short protection function built inside.
9.3 Tab connection
Ultrasonic welding or spot welding is recommended to connect battery with PCM or
other parts.
If apply manual solder method to connect tab with PCM, the notice below is very
important to ensure battery performance.
⑴
The electric iron should be temperature controlled and ESD safe;
⑵ Soldering temperature should not exceed 350
℃
;
⑶ Soldering time should not be longer than 3s, keep battery tab cold down before next
soldering;
⑷
Soldering times should not exceed 5 times;
⑸
Directly heat cell body is strictly prohibited, battery may be damaged by heat above
approx. 100
℃.
9.4 Cell fixing
The battery should be fixed to the battery pack by its large surface area. No cell
movement in the battery pack should be allowed.
9.5 Cells replacement
The cell replacement should be done by professional people.
Prohibit short-circuit between cells’ Al package and exterior component.