Operating Manual

141
Fig. 15-10. Radiograph of an aluminium casting with coarse porosity
Exposure on D7 film at 60 kV/5 mA/15 sec, film-focus distance 100 cm
140
Fig. 15-8. Hot cracks (hot tears)
Fig. 15-9. Stress cracks (cold tears)