Fig. 15-3. Shrinkage (worm-hole cavities) in a (high heat conductive) copper casting
136
Fig. 15-2. Radiograph of an aluminium precision casting. Exposure on D2 film at 75 kV/5 mA/3.5 min/film-focus distance 100 cm