MSDS
GREAT POWER BATTERY
MATERIAL SAFETY DATA SHEET
No.:PH-MSDS-2014
Date:Jan/01/2014
1. Identification of the substance/preparation and of the company/undertaking
Identification of the product
Product name:
Chemical System:
Model:
Designated for RECHARGE?
Polymer Li-ion Battery
LiCoO2/C
Prismatic Type Cells
X Yes __ No
Manufacturer/supplier identification
Company:
GREAT POWER BATTERY(ZHUHAI)CO., LTD.
Contact for information:
XINQING 5
th
RD. , DOUMEN DISTTICT, ZHUHAI
GD, PRC
Emergency telephone No.:
0086-13726243449 Michael@greatpower.net
2. Composition/information on ingredients
Ingredient
Percent
CAS Index
No./EC No.
Molar
mass
Molecular
formula
Symbol
Lithium cobaltate
31.6%
12190-79-3
LiCoO2
Graphite
17.1%
7782-42-5
C
Organic Electrolyte
13.2%
21324-40-3
Polypropylene
2.8%
9003-07-0
Copper foil
6.5%
7440-50-8
Cu
Aluminum
28.8%
7429-90-5
Al
Weight of lithium per cell: 0g. There is no metallic lithium in the polymer Li-ion battery.
3. Hazards identification
Health Hazards (Acute and Chronic):
For the battery cell, chemical materials are stored in a hermetically sealed aluminum laminate case, designed to
withstand temperatures and pressures encountered during normal use. As a result, during normal use, there is no
physical danger of ignition or explosion and chemical danger of hazardous materials leakage.
However, if exposed to a fire, added mechanical shocks, decomposed, or added electric stress by misuse the cell
case will be breached and hazardous materials may be released. Moreover, if heated strongly by the surrounding
fire, acrid gas may be emitted.
Carcinogenicity:
NTP: None IARC Monograph: None OSHA Regulated: None
Medical Conditions Generally Aggravated by Exposure:
An acute exposure will not generally aggravate any medical condition.
Human health effects:
Inhalation: The steam of the electrolyte has an anesthesia action and stimulates a respiratory tract.
Skin contact: The steam of the electrolyte stimulates a skin. The electrolyte skin contact causes a sore and the