SDS

SAMSUNG SDI Co., Ltd.
Date: Jan 7
th
2020 Revision no.: 01
ELG(P11P35-11-N01,3.7L1200SPA)
Page 3 of 22
exposure occurs only if the cell or pack is mechanically, thermally, electrically or physically abused to the
point of compromising the enclosure.
If this occurs, exposure to the electrolyte solution contained within can occur by inhalation, ingestion, eye
contact and skin contact.
Potential Health Effect(s):
Acute (short term): see Section 8 for exposure controls.
In the event that this cell or pack has been ruptured, the electrolyte solution contained within the cell
would be corrosive and can cause burns to skin and eyes.
Inhalation: Inhalation of materials from a sealed cell is not an expected route of exposure. Vapors
or mists from a ruptured cell may cause respiratory irritation.
Ingestion: Swallowing of materials from a sealed cell is not an expected route of exposure.
Swallowing the contents of an open cell can cause serious chemical burns to mouth, esophagus,
and gastrointestinal tract.
Skin: Contact between the cell and skin will not cause any harm. Skin contact with the contents of
an open cell can cause severe irritation or burns to the skin.
Eye: Contact between the cell and the eye will not cause any harm. Eye contact with the contents of
an open cell can cause severe irritation or burns to the eye.
CHRONIC (long term): see Section 11 for additional toxicological data.
Interactions with other chemicals: Immersion in high conductivity liquids may cause corrosion and
breaching of the cell or battery enclosure. The electrolyte solution inside of the cells may react with
alkaline (basic) materials and present a flammability hazard.
Potential Environmental Effects: Not Available.
Section III COMPOSITION/INFORMATION ON INGREDIENTS
3.1 Mixture
Chemical Name
CAS No.
*Mass range in cell (g/g %)
Lithium Cobalt Oxide (CoLiO2)
12190-79-3
30~50
Graphite
7782-42-5
20~25
Iron
7439-89-6
10~15
Copper
7440-50-8
5~10
Aluminum
7429-90-5
5~10
Dimenthyl carbonate
616-38-6
0.1~5
Carbonate, methyl ethyl
623-53-0
0.1~5
Further Information
Because of the cell structure the dangerous ingredients will not be available if used properly.
During charge process a lithium graphite intercalation phase is formed.