SDS

SAMSUNG SDI Co., Ltd.
Date: January 1, 2018 Reference no.: SDI-TTi-30T-I-1
MODEL: INR21700-30T Revision no.: 00
Page 4 of 11
Acute (short term): see Section 8 for exposure controls.
In the event that this cell or pack has been ruptured, the electrolyte solution contained within the cell would
be corrosive and can cause burns to skin and eyes.
Inhalation: Inhalation of materials from a sealed cell is not an expected route of exposure. Vapors or mists
from a ruptured cell may cause respiratory irritation.
Ingestion: Swallowing of materials from a sealed cell is not an expected route of exposure. Swallowing the
contents of an open cell can cause serious chemical burns to mouth, esophagus, and gastrointestinal tract.
Skin: Contact between the cell and skin will not cause any harm. Skin contact with the contents of an open
cell can cause severe irritation or burns to the skin.
Eye: Contact between the cell and the eye will not cause any harm. Eye contact with the contents of an open
cell can cause severe irritation or burns to the eye.
CHRONIC (long term): see Section 11 for additional toxicological data.
Interactions with other chemicals: Immersion in high conductivity liquids may cause corrosion and breaching of
the cell or battery enclosure. The electrolyte solution inside of the cells may react with alkaline (basic) materials
and present a flammability hazard.
Potential Environmental Effects: Not Available.
3. Composition/information on ingredients
Hazardous components
Chemical Name
CAS No.
*Mass range in cell (g/g %)
Electrolyte
Contains Electrolyte salt and solvents.
5-20
Electrolyte salt
Lithium hexafluorophosphate
21324-40-3
0.05-5
Electrolyte
solvent
Includes one or more of the following;
Ethelyne Carbonate
Propylene Carbonate
Diethyl Carbonate
Ethyl propionate
96-49-1
108-32-7
105-58-8
105-37-3
5-20
PVDF
Polyvinylidenfluoride
24937-79-9
<1
Copper
Cu
7440-50-8
3-15
Aluminium
Al
7429-90-5
2-10
Cathode
Lithium cobalt oxide
12190-79-3
20-50
Anode
Graphite
7782-42-5
10-30
Steel, Nickel, and
inert components
Various Balance
Because of the cell structure the dangerous ingredients will not be available if used properly.
During charge process a lithium
graphite intercalation phase is formed.
4. First Aid Measures
Description of first aid measures
The hazardous components of this cell or battery are contained within a sealed unit. The following measures are only
applicable if exposure has occurred to components when a cell or battery leaks, is exposed to high temperatures or is