How to Guide
TECHNICAL DATA
S71 WATER-BASED EPOXY PRIMER
Form: GDH-985
Rev.: 102915
2
.PERFORMANCE CHARACTERISTICS .
PENCIL HARDNESS
METHOD: ASTM D3363
RESULT: 3H
CONICAL FLEXIBILITY
METHOD: ASTM D522
RESULT: 180°, ½"
CYCLIC PROHESION
Rating 1-10 10=best
METHOD: ASTM D5894, 1 cycle, 336 hours
RESULT: 10 per ASTM D714 for blistering
RESULT: 10 per ASTM D1654 for corrosion
RESULT: 10 per ASTM D610 for rusting
IMPACT RESISTANCE (direct)
METHOD: ASTM D2794
RESULT: 50 in. lbs.
INTERCOAT ADHESION
METHOD: ASTM D3359
RESULT: Excellent
CORROSION RESISTANCE
METHOD: ASTM B117, Salt Spray, CRS B1000
RESULT: 4 mils 1800 hours
HUMIDITY RESISTANCE
METHOD: ASTM D4585
RESULT: CRS B1000 4 mils, 1300 hours
For chemical and corrosion resistance, see the
Rust-Oleum Industrial Brands Catalog (Form #275585).