Instructions / Assembly

- 12 -
reddening during the welding process and cause the flux skin to fall off,
affecting the quality of welding.
3. Connection method of welding output
The DC reverse connection method should be used for alkaline
electrode welding.
Acid electrode welding should use a DC positive connection method.
Hot Stapler
1. Select "Hot stapler" via the up and down button. In "Hot Stapler" mode,
the Vrd light will be on automatically, and all other functions are not
adjustable except "Current".
2. Adjust the gear of the plastic welding through the knob, and select the
corresponding 1 or 2 gears according to the thickness of the welding
material.
3. Press the switch button on the grip and hold for about 3 seconds until
the pin is hot enough to weld.
Then press the pin gently against the desired repair location.
WHEN THE HEATING REPAIR PIN IS PRESSED TOO HARD, IT
MAY PENETRATE THE OBJECT. PLEASE PRESS LIGHTLY.
4. When the pin is taken halfway to the repairing part, release the switch
button on the grip, then wait for a few seconds until the repair part
becomes firm. After that, draw the pin out of the grip.
5. When a repairing part reaches long and wide, please repeat the
procedure 5 ~ 7 at intervals of 1 ~ 3cm.
6. Cut off the pin using pliers.