To avoid stress cracking, do not use square-cut inside corners. All inside corners should have a
minimum of 1/8” (3.175mm) radius and all edges should be routed smooth.
Drill oversized holes for screws or bolts. Screws or bolts should be slightly countersunk into the face
side of a laminate-clad substrate.
Take care to ensure an appropriate acclimation between the laminate and the substrate prior to
fabrication. The face and backing laminates and the substrate should be conditioned in the same
environment for 48 hours before fabrication.
Recommended conditioning temperature is about 75°F (24°C). Laminates should be conditioned at
45% to 55% relative humidity.
With postforming machinery, Wilsonart 362/367 and 372/377 will postform at a nominal sheet
temperature range of 325°F to 350°F (163°C to 176°C) in 20 ± 5 seconds.
Carbide-tipped saw and router blades should be used for cutting. High tool speed and low feed speed
are advisable. Cutting blades should be kept sharp. Use a hold-down to prevent any vibration.
5. Warranty
6. Maintenance
7. Technical Services
For samples, literature, questions or technical assistance, please contact our toll-free Hotline at (800)
433-3222, Monday through Friday, 8 am – 5 pm, CST.
Specification Form
Surface shall be Wilsonart Virtual Design Library Laminate, produced by Wilsonart LLC,
Temple, Texas 76503-6110
Type: Specify 362, 367, 372 or 377
Surface
Color Number: _____________ Color Name: ______________
Finish
Number: _____________ Name: ______________
Edge Trim
Color Number: _____________ Color Name: ______________
Adhesive
Name: _____________ Grade/Type: __________
Brand: Wilsonart® Adhesive
Wilsonart® VDL Laminate Technical Data
Revised: September 8, 2017
© 2017, Wilsonart LLC